IS 12654:1989 provides a comprehensive code of practice for the preparation and use of calcined low-grade gypsum in the building industry. It specifies physical requirements, preparation methods, and applications of gypsum plaster, mortar, and lightweight gypsum blocks primarily for internal plastering, masonry mortar, and non-load bearing walls. This standard is essential for engineers and builders aiming to utilize abundant low-grade gypsum resources in India, especially for cost-effective construction solutions.
نظرة عامة
IS 12654:1989 provides a comprehensive code of practice for the preparation and use of calcined low-grade gypsum in the building industry. It specifies physical requirements, preparation methods, and applications of gypsum plaster, mortar, and lightweight gypsum blocks primarily for internal plastering, masonry mortar, and non-load bearing walls. This standard is essential for engineers and builders aiming to utilize abundant low-grade gypsum resources in India, especially for cost-effective construction solutions.
الجمهور
المحتويات
الهيكل
IS 12654: Scope - Key Dimensions and Tolerances
| Dimension | Size (mm) |
|---|---|
| Length | 700 max, in multiples of 100 |
| Breadth | 75, 100, 125, 150 |
| Height | 300 max, in multiples of 100 |
Rounding Off (Clause 8.2):
Values from tests or calculations must be rounded as per IS 2:1960 rules, retaining the same significant figures as specified.
Physical Requirements (Clause 8.4):
Specifies mandatory physical properties (not detailed here) to ensure block quality.
flowchart TD
A[IS 12654 Scope] --> B[Dimensions & Tolerances]
B --> C[Length: ≤700 mm, multiples of 100]
B --> D[Breadth: 75, 100, 125, 150 mm]
B --> E[Height: ≤300 mm, multiples of 100]
A --> F[Rounding: IS 2:1960]
A --> G[Physical Requirements]
This ensures uniformity and quality control for blocks under IS 12654.
Key Indian Standards Adjunct to IS 12654 (Clause 2.1):
| IS No. | Title | Year |
|---|---|---|
| IS 1288 | Methods of test for mineral gypsum | 1982 |
| IS 2250 | Code of practice for preparation and use of masonry mortars | 1981 |
| IS 2469 | Glossary of terms relating to gypsum | 1976 |
| IS (1/Sec 1-12) | Methods of test for gypsum plaster, concrete and products: Part 1 Plaster and concrete | 1978 |
| IS 2542 (Part 2/Sec 1-8) | Methods of test for gypsum plaster, concrete and products: Part 2 Gypsum products | 1981 |
| IS 8272 | Specification for gypsum plaster for use in manufacture of fibrous plaster boards | 1984 |
| Dimension | Nominal Size (mm) | Notes |
|---|---|---|
| Length | 700 (max) | In multiples of 100 mm |
| Breadth | 75, 100, 125, 150 | |
| Height | 300 (max) | In multiples of 100 mm |
flowchart TD
A[IS 12654] --> B[IS 1288 - Mineral Gypsum Tests]
A --> C[IS 2250 - Masonry Mortars]
A --> D[IS 2469 - Gypsum Glossary]
A --> E[IS 1/Sec 1-12 - Gypsum Plaster Tests]
A --> F[IS 2542
IS 12654 - Definitions: Key Specifications and Dimensions
| Dimension | Value (mm) | Notes |
|---|---|---|
| Length | 700 max | In multiples of 100 mm |
| Breadth | 75, 100, 125, 150 | Standard breadth options |
| Height | 300 max | In multiples of 100 mm |
flowchart TD
A[Block Dimensions] --> B{Length}
B -->|Max 700 mm| C[Multiples of 100 mm]
A --> D{Breadth}
D -->|75, 100, 125, 150 mm| E[Standard Sizes]
A --> F{Height}
F -->|Max 300 mm| G[Multiples of 100 mm]
This ensures uniformity and interchangeability of blocks as per IS 12654.
Purity of Gypsum (IS 12654)
| Parameter | Requirement | Test Reference |
|---|---|---|
| Fineness (passing 150 micron sieve) | Minimum 95% | Annex A |
| Setting Time | 10 to 30 minutes | IS 2542 (Part 1/Sec 1 to 12):1978 |
| Compressive Strength | Minimum 7.0 N/mm² | IS 8272:1984 (Appendix D) |
flowchart LR
A[Raw Gypsum] --> B[Purity Test (IS 1288)]
B -->|≥ 60% CaSO4·2H2O| C[Acceptable for Use]
B -->|< 60%| D[Reject or Process Further]
C --> E[Preparation of Calcined Gypsum]
E --> F[Gypsum Plaster Production]
This ensures quality gypsum plaster conforming to IS 12654 standards.
IS 12654: Preparation of Calcined Gypsum (Gypsum Plaster)
Gypsum plaster must conform to Table 1 (physical and chemical properties). Typical parameters include:
| Property | Requirement |
|---|---|
| Setting time | Initial: 30-45 min; Final: < 60 min |
| Fineness | 90% passing 90-micron sieve |
| Soundness (expansion) | ≤ 3 mm |
| Compressive strength | ≥ 1.5 MPa (after 7 days) |
| Loss on ignition | ≤ 10% |
flowchart LR
A[Low-grade Gypsum] --> B[Calcination (150-180°C)]
B --> C[Calcined Gypsum (Plaster)]
C --> D{Uses}
D --> E[Masonry Mortar]
D --> F[Internal Plaster]
D --> G[Lightweight Blocks]
This summarizes key preparation and quality criteria per IS 12654. For detailed Table 1 values, refer to the standard document.
IS 12654: Physical Requirements Summary
| Dimension | Value (mm) | Notes |
|---|---|---|
| Length | 700 max | In multiples of 100 mm |
| Breadth | 75, 100, 125, 150 | Standard widths |
| Height | 300 max | In multiples of 100 mm |
Nominal Dimensions (mm):
- Length ≤ 700 (multiples of 100)
- Breadth = 75, 100, 125, or 150
- Height ≤ 300 (multiples of 100)
Tolerances:
- Length & Breadth: ±3 mm
- Height: ±5 mm
This ensures blocks are consistent for masonry work, aiding structural integrity and aesthetics.
IS 12654: Key Details on Gypsum Mortar
| Component | Proportion (by mass) | Notes |
|---|---|---|
| Gypsum Plaster | 1 | Conforms to Table 1 |
| Sand | 2 | Clean, well-graded |
| Water | 50% of total mass | For workable consistency |
flowchart TD
A[Gypsum Plaster] --> C[Gypsum Mortar Mix]
B[Sand] --> C
D[Water (50%)] --> C
C --> E[Apply on Clean, Wetted Brick Surface]
E --> F[Set for 48 Hours]
F --> G{Check for Defects}
G -->|No cracks, chalking, peeling| H[Acceptable Mortar]
G -->|Defects Present| I[Reject or Rework]
This ensures gypsum mortar meets IS 12654 durability and application standards.
IS 12654: Light Weight Solid Gypsum Blocks for Non-Load Bearing Walls
| Property | Requirement |
|---|---|
| Compressive Strength | Typically ≥ 3.5 MPa |
| Density | Around 700 - 1000 kg/m³ |
| Water Absorption | ≤ 15% |
| Dimensions | As per IS standard sizes (e.g., 600x200x100 mm) |
[ \text{Gypsum Mortar} = 1 \times \text{Gypsum Plaster} + 2 \times \text{Sand} + 0.5 \times \text{Water (mass fraction)} ]
flowchart LR
A[Calcined Gypsum] --> B[Light Weight Solid Blocks]
B --> C[Non-Load Bearing Walls]
A --> D[Gypsum Mortar]
D --> E[1 part Gypsum + 2 parts Sand + 50% Water]
E --> F[Internal Plastering & Masonry]
Note: Always verify block dimensions and strength from supplier certificates as per IS 12654.
IS 12654: Method for Determination of Fineness of Gypsum Blocks
| Step | Procedure |
|---|---|
| 1 | Take 100 g of dried gypsum sample |
| 2 | Sieve continuously on a 150 µm IS sieve for 5 minutes |
| 3 | Break air-set lumps gently by fingers (no rubbing on sieve) |
| 4 | Weigh material retained on sieve |
| 5 | Calculate fineness as: |
[ \text{Fineness (% passing)} = 100 - \left(\frac{\text{Mass retained on 150 µm sieve}}{100}\times 100\right) ]
flowchart TD
A[100 g dried sample] --> B[Sieve on 150 µm IS sieve for 5 min]
B --> C[Break lumps gently]
C --> D[Weigh retained material]
D --> E[Calculate % passing = 100 - (retained mass %)]
E --> F{Is fineness ≥ 95%?}
F -- Yes --> G[Sample passes fineness test]
F -- No --> H[Sample fails fineness test]
This ensures gypsum plaster quality per IS 12654.
الأسئلة المتكررة
According to IS 12654, Clause 4.1, the minimum purity requirement for low-grade gypsum is:
| Parameter | Requirement |
|---|---|
| Purity of CaSO₄·2H₂O | ≥ 60% |
| Test Method | IS 1288:1982 |
| Common Impurities | Silica, Dolomite, Carbonates |
This ensures the gypsum is adequate for calcination and plaster production under the code of practice.
Calcination of Low-Grade Gypsum as per IS 12654
Note: Low-grade gypsum with purity ≥60% CaSO4·2H2O can be effectively calcined for plaster and blocks.
جارٍ تحميل المخطط…
Recommended Mix Proportions for Gypsum Mortar (IS 12654)
Application Notes:
جارٍ تحميل المخطط…
This ensures a durable, workable mortar conforming to IS 12654 standards.
According to IS 12654 and related studies by CBRI:
| Application | Use of Low-Grade Gypsum Blocks |
|---|---|
| Internal Non-Load Bearing Walls | Suitable |
| External Walls (Exposed) | Not recommended (except very dry climate) |
Therefore, gypsum blocks from low-grade gypsum should not be used for external walls exposed to weather. They are best suited for internal partitions in low-cost housing.
جارٍ تحميل المخطط…
Compressive Strength Requirements as per IS 12654:
Gypsum Mortar (Clause 7.4.2 & 2.5):
Lightweight Solid Gypsum Blocks (Clause 8 & 1.5):
Additional Notes:
جارٍ تحميل المخطط…
اسأل AI عن أي بند، متطلب، أو حكم في IS 12654. احصل على ردود فورية مع الاستشهاد بالبند مدعومة بمكتبتنا المفهرسة.
الطبقة المجانية تشمل 150 استعلامًا (50 AI + 100 مرجعي) · لا حاجة لبطاقة ائتمان