IS 71981974AI Search Enabled✦ AI Generated

IS 7198 — Code of practice for damp-proofing using bitumen mastic

IS 7198:1974 provides a comprehensive code of practice for damp-proofing buildings using bitumen mastic. It covers the application procedures for preventing water penetration and rising damp in both below-ground and above-ground structures, including walls, floors, and foundations. This standard is essential for engineers and construction professionals involved in waterproofing and damp-proofing works using bitumen mastic in reinforced concrete, masonry, and steel structures.

12Sections
44Clauses Indexed
✓AI Search Ready
1974Edition
Waterproofing and Damp-ProofingCategory
Alternative search terms: IS 7198 PDF, IS 7198 pdf free download, IS 7198 free download pdf, IS7198 PDF, IS-7198 PDF, IS 7198 1974 PDF, IS 7198:1974 PDF, IS 7198-1974 PDF, IS 7198 (1974) PDF, IS 7198 1974 edition PDF, IS 7198 edition 1974 PDF

What This Standard Covers

IS 7198:1974 provides a comprehensive code of practice for damp-proofing buildings using bitumen mastic. It covers the application procedures for preventing water penetration and rising damp in both below-ground and above-ground structures, including walls, floors, and foundations. This standard is essential for engineers and construction professionals involved in waterproofing and damp-proofing works using bitumen mastic in reinforced concrete, masonry, and steel structures.

Who Uses This Standard

  • Civil Engineers
  • Structural Engineers
  • Waterproofing Specialists
  • Construction Project Managers
  • Architects
  • Quality Control Inspectors
  • Building Contractors

Key Topics Covered

✓Scope and application of bitumen mastic for damp-proofing
✓Types of structures suitable for treatment
✓Surface preparation and site conditions
✓Materials specifications including bitumen mastic requirements
✓Method of mixing and remelting bitumen mastic
✓Thickness and layering techniques for vertical and horizontal surfaces
✓Application procedures for below-ground and above-ground damp-proofing
✓Details on joints, chases, and angle fillets
✓Precautions for internal and external tanking
✓Load considerations and allowable stresses
✓Continuity and protection of damp-proof membranes
✓Treatment around service openings and penetrations

Table of Contents

1Scope▼

IS 7198: Scope - Key Points & Specifications

Scope (Clause 2.1):

  • Design must follow basic info as per IS 3067-1966 for efficient design and construction of bitumen mastic tanking.

General Considerations (Clause 6.1.1):

  • Ensures proper design methodology and construction practices are followed.

Thickness & Laying Method (Clause 8.5):

  • Construction joints:
    • Warm edges of laid mastic with hot asphalt.
    • Remove dust/dirt by cutting with a metal trowel.
    • Pour fresh mastic before surface cools.

Mixing Method (Clause 7.1):

  • Follow IS 5871-1970 for mixing bitumen mastic.

Typical Structural Form (Fig. 4)

LayerThickness/Notes
Cement Sand Protective Screed5 cm thick
Bitumen Mastic Angle FilletAs per design
Lean Base ConcreteAs per site requirement
Working Platform (Rubble Soling, Rammed Earth, etc.)Provides stable base

Summary Table: Thickness & Laying

Layer/OperationSpecification/Action
Protective Screed5 cm cement-sand
Construction JointsWarm, clean, pour fresh mastic immediately
MixingIS 5871-1970 compliant method

flowchart TD
    A[Working Platform] --> B[Lean Base Concrete]
    B --> C[Bitumen Mastic Angle Fillet]
    C --> D[Cement Sand Protective Screed (5 cm)]

For detailed design and construction, refer to IS 3067-1966, IS 5871-1970, and IS 7198 clauses above.

2Necessary Information for Design and Construction Work for Damp-Proofing▼

IS 7198: Key Specifications & Guidelines for Damp-Proofing Design and Construction

1. Applicable Structures (Clause 1.2)

  • Reinforced concrete, prestressed concrete, plain concrete (special cases)
  • Dense concrete, blockwork, plastered brick or stone masonry
  • Structural steel with other materials

2. Damp-Proofing for Walls and Floors Above Ground (Clause 6.1.2 & 5.2)

  • DPC shall cover full thickness of walls (excluding plaster) or base of cavity walls.
  • No setback for pointing; must be continuous with bitumen mastic layer in adjacent floors.
  • Vertical DPC may be provided on the inner surface where necessary.
  • DPC height: minimum 150 mm above ground level.

3. Surface Preparation & Laying (Clause 6.1.1.6)

  • Keep surface dry during laying.
  • Follow IS 3067-1966 for laying bitumen mastic.
  • Maintain dewatering until bitumen layers harden and structure gains strength to resist hydrostatic pressure.

4. Typical Arrangement (Fig. 2)

flowchart TB
    A[Periphery Wall (Hollow)] --> B[Damp-proof Course (Full Thickness)]
    B --> C[Bitumen Mastic Layer in Floor]
    C --> D[Lean Base Concrete]
    D --> E[Floor Concrete]

Summary Table: DPC Specifications

ParameterSpecification
DPC LocationFull wall thickness (excluding plaster)
DPC Height Above Ground≥ 150 mm
ContinuityContinuous with bitumen mastic in floor
Surface ConditionDry, dewatered during laying
Reference StandardIS 3067-1966 (Bitumen mastic laying)

This ensures effective damp-proofing integrated with structural elements.

3Materials▼

IS 7198 — Materials Key Points

  1. Bitumen Mastic:

    • Must conform to IS 5871-1970 (Specification for bitumen mastic for tanking and damp-proofing).
    • Mixing method as per Clause 7.1 follows IS 5871-1970.
  2. Design Information:

    • Basic design data should comply with IS 3067-1966 (Clause 2.1).
  3. Construction Joints (Clause 8.5):

    • Edges of laid mastic warmed with hot asphalt.
    • Remove dust/dirt by cutting with metal trowel.
    • Fresh mastic poured before the joint surface cools.
  4. Typical Structural Form (Fig. 4):

    • 5 cm thick cement-sand protective screed
    • Bitumen mastic angle fillet
    • Lean base concrete
    • Hard working platform (rubble soling, rammed earth)

Summary Table: Bitumen Mastic Properties (from IS 5871-1970)

PropertyRequirement
Penetration (dmm)40-90 (at 25°C)
Softening Point (°C)Min. 80
Ductility (cm)Min. 10
Solubility (%)Min. 99

Construction Joint Preparation (Clause 8.5)

flowchart LR
    A[Existing Mastic Edge] --> B[Warm with Hot Asphalt]
    B --> C[Cut & Remove Dust/Dirt]
    C --> D[Pour Fresh Mastic Before Cooling]

References:

  • IS 5871-1970 for bitumen mastic specs and mixing.
  • IS 3067-1966 for design data.
  • Use protective screed and proper base layers for durability.
4Allowable Loads▼

IS 7198: Allowable Loads Summary

  • Clause 4.1: When bitumen mastic is not properly compacted to prevent extrusion, the maximum design load should not exceed:

    [ \boxed{ 6.5 \text{ kgf/cm}^2 } ]

    at maximum atmospheric temperature.

  • Proper compaction is critical to ensure mastic integrity and allow higher loads.

  • For design, refer to IS 3067-1966 Clause 2.1 for basic information on load considerations.


Key Points:

ParameterValueNotes
Max allowable load (improper compaction)6.5 kgf/cm²At max atmospheric temperature
Bitumen mastic standardIS 5871-1970For material conformity

Practical Advice:

  • Ensure proper compaction of bitumen mastic to maximize allowable load.
  • For design loads beyond 6.5 kgf/cm², verify compaction quality and consult IS 3067 for detailed design data.
flowchart TD
    A[Bitumen Mastic] --> B{Properly Compacted?}
    B -- Yes --> C[Allow Higher Loads]
    B -- No --> D[Limit Load to 6.5 kgf/cm²]
    C --> E[Design According to IS 3067]
    D --> E

This ensures safe design respecting IS 7198 provisions.

5Location of Damp-Proofing Treatment▼

Location of Damp-Proofing Treatment (IS 7198)

Key Specifications:

  • Walls and Floors Above Ground (Clause 6.1.2):

    • Damp-proofing must cover the full thickness of walls, excluding plaster.
    • For cavity walls, apply at the base of the cavity.
    • No setback for pointing is allowed.
    • Must be continuous with bitumen mastic layer in adjacent floors.
    • Provide a vertical damp-proof course on the inner wall surface if necessary (see Fig. 2).
  • Height Above Ground (Clause 5.2):

    • Damp-proof course (DPC) should extend to at least 150 mm above ground level.
  • Load Limitation (Clause 4.1):

    • If bitumen mastic is not properly compacted, max design load ≤ 6.5 kgf/cm² at max atmospheric temperature.

Typical Arrangement (Fig. 2)

graph TB
    A[Periphery Wall (Hollow)] --> B[Damp-proofing across full thickness]
    B --> C[Continuous with Bitumen Mastic on Floor]
    C --> D[Floor Concrete]
    D --> E[Lean Base Concrete]

Summary Table

ParameterSpecification
DPC thicknessFull wall thickness excl. plaster
DPC height above ground≥ 150 mm
Max design load on mastic≤ 6.5 kgf/cm² (if not compacted)
ContinuityMust link wall and floor DPC

This ensures effective moisture barrier preventing rising damp and water ingress.

6Preparation of Surface and Site for Damp-Proofing▼

IS 7198: Preparation of Surface and Site for Damp-Proofing

Key Specifications & Requirements

  • Damp-proof course (DPC) height: At least 150 mm above ground level (Clause 5.2).
  • Surface condition: Must be clean, dry, and free of dirt/dust before laying bitumen mastic (Clause 6.1.1.2).
  • Dewatering: Continuous dewatering is essential during laying and until bitumen mastic hardens and structure gains strength (Clause 6.1.1.6).
  • Continuity: DPC must be continuous across full wall thickness (excluding plaster) and continuous with adjacent floor bitumen mastic layers (Clause 6.1.2).

Preparation Steps (Summary)

  • Clean surface thoroughly.
  • Ensure surface dryness.
  • Maintain dewatering to prevent hydrostatic pressure buildup.
  • Lay damp-proofing continuously without setbacks, including vertical DPC on inner wall surfaces.

Typical Arrangement (Fig. 2)

flowchart TB
    A[Lean Base Concrete] --> B[Floor Concrete]
    B --> C[Bitumen Mastic Layer]
    C --> D[Periphery Hollow Wall]
    D --> E[Vertical DPC on Inner Surface]

Reference Standards

  • IS 3067-1966: Dewatering and preparatory work.
  • Specification for bitumen mastic for tanking and damp-proofing.

This ensures effective moisture barrier and structural integrity against dampness.

7Method of Mixing and Remelting▼

IS 7198 - Method of Mixing and Remelting Bitumen Mastic

1. Method of Remelting (Clause 7.2)

  • Use a mechanical mixer on-site.
  • Stock broken bitumen mastic blocks (per IS 5871-1970) in layers around mixer sides, then towards center.
  • Gradually heat to ~200°C; do not exceed 200°C to avoid property degradation.
  • Continuous agitation ensures uniform consistency.
  • Total heating duration and plant type must preserve bitumen mastic properties.

2. Method of Mixing (Clause 7.1)

  • Follow the procedure in IS 5871-1970 (Specification for bitumen mastic for tanking and damp-proofing).
  • Clean surface thoroughly before application (Clause 6.1.1.2).

3. Protective Measures (Clause 6.1.4)

  • Provide 300 mm clearance outside walls during excavation.
  • Apply 50 mm thick cement-sand screed (1:4 ratio) after laying horizontal mastic and angle fillets.
  • Allow mastic coats to harden before backfilling.

Summary Table: Remelting Parameters

ParameterValue/Specification
Max Temperature200°C
Heating MethodMechanical mixer, gradual heat
AgitationContinuous during melting
Bitumen Mastic SourceBlocks conforming to IS 5871-1970
Protective ScreedCement:Sand = 1:4, Thickness = 50 mm
flowchart TD
    A[Bitumen Mastic Blocks] --> B[Stock in layers in mixer]
    B --> C[Gradual heating to 200°C]
    C --> D[Continuous agitation]
    D --> E[Uniform melted bitumen mastic]

This ensures uniform mixing and maintains bitumen mastic quality per IS 7198 requirements.

8Thickness and Method of Laying▼

IS 7198: Thickness & Method of Laying of Bitumen Mastic

Key Specifications (Clause 8)

  • Number of coats: 3 (vertical, horizontal, or sloping surfaces)
  • First coat: Thin, acts as adhesive & prevents blowing.
  • Subsequent coats: Spread evenly and uniformly with a float.
  • Vertical surfaces: First coat plastered with metal trowel; 2nd & 3rd coats with wooden float.
  • Timing: Apply next coat ASAP to avoid dust/dirt accumulation affecting adhesion.

Thickness (from Clause 8.5 Table summary)

Surface TypeTotal Thickness (mm)Notes
HorizontalTypically 10-15 mmSpread evenly with float
VerticalTypically 8-12 mmFirst coat thin, others uniform

Construction Joints (Clause 8.5)

  • Warm edges of laid mastic with hot asphalt.
  • Cut edges with metal trowel to remove dust/dirt.
  • Pour fresh mastic before joint surface cools.

Method of Remelting (Clause 7.2)

  • Remelt bitumen mastic in mechanical mixer at site.
  • Heat gradually to ~200℃; do not exceed 200℃.
  • Continuous agitation for uniform consistency.

Summary Diagram (Laying Process)

flowchart TD
    A[Prepare Surface] --> B[Apply 1st Coat Thinly]
    B --> C{Surface Type}
    C -->|Horizontal| D[Spread with Float]
    C -->|Vertical| E[Plaster with Metal Trowel]
    D --> F[Apply 2nd & 3rd Coats with Wooden Float]
    E --> F
    F --> G[Ensure Uniform Thickness]
    G --> H[Apply Next Coat ASAP]
    H --> I[Finish with Construction Joints Treatment]

This ensures proper adhesion, uniform thickness, and durability of bitumen mastic as per IS 7198.

9Precautions for Internal and External Tanking▼

IS 7198: Precautions for Internal & External Tanking


External Tanking (Clause 6.1.3)

  • Working space outside walls: ≥ 0.6 m
  • Base: Structurally sound, even thickness ≥ 100 mm, extended ≥ 150 mm beyond wall edges for angle fillet.
  • Protection:
    • Cover horizontal mastic asphalt immediately with 50 mm cement-sand screed.
    • Protect angle fillet (150 mm bitumen mastic) with 50 mm cement-sand screed over building paper.
    • After vertical damp-proofing, erect a brick wall (10 cm thick) outside for protection.
  • Fig. 3 illustrates layering:
    Brick wall → Cement-sand screed (5 cm) → Structural form → Base → Hard working platform.

Internal Tanking (Clause 6.1.4)

  • Excavation space: ≥ 300 mm outside wall to keep dry.
  • Base slab: Even surface for damp-proofing.
  • Walls: Built full height before mastic application.
  • Earth filling: Only after 3 vertical mastic coats & hardened loading coats.
  • Protection: After horizontal mastic & angle fillets, apply 50 mm cement-sand (1:4) screed before structural floor/walls.
  • Fig. 4 layering:
    Cement-sand screed (5 cm) → Bitumen mastic angle fillet → Lean base concrete → Hard working platform.

Additional Notes

  • Openings: Avoid openings in tanked walls/floors; if necessary, provide special treatment (Fig. 1).
  • Mixing: Follow IS 5871-1970 for bitumen mastic mixing/remelting.

Summary Table

ParameterExternal TankingInternal Tanking
Working space outside wall≥ 0.6 m≥ 0.3 m
Base thickness≥ 100 mmEven surface (min 100 mm)
Base extension beyond wall≥ 150 mmNot specified
Protective screed thickness50 mm cement-sand50 mm cement-sand (1:4)
10Details of Joints, Chases, and Angle Fillets▼

IS 7198 Key Specifications for Joints, Chases, and Angle Fillets

1. Joints (Clause 8.2.2 & 8.5)

  • Joints in successive bitumen mastic coats must be staggered:
    • Horizontal: ≥ 150 mm
    • Vertical: ≥ 75 mm
  • Construction joints:
    • Warm edges of existing mastic with hot asphalt.
    • Clean and cut with metal trowel.
    • Pour fresh mastic before surface cools.

2. Chases (Clause 8.3)

  • Vertical bitumen mastic top should turn into a chase of minimum 25×25 mm unless continuing horizontally.

3. Angle Fillets (Clause 8.4)

  • Apply angle fillet at internal junctions.
  • Minimum width: 50 mm.
  • Apply in two coats.

Summary Table:

FeatureDimension/Specification
Joint StaggeringHorizontal ≥ 150 mm, Vertical ≥ 75 mm
Chase SizeMinimum 25 mm × 25 mm
Angle Fillet WidthMinimum 50 mm, two coats

flowchart LR
    A[Joints] --> B[Staggered: Horizontal ≥150 mm]
    A --> C[Staggered: Vertical ≥75 mm]
    A --> D[Warm & clean edges before fresh mastic]

    E[Chases] --> F[Vertical chase: 25×25 mm min]

    G[Angle Fillets] --> H[Min width 50 mm]
    G --> I[Apply in two coats]

This ensures durability and proper bonding of bitumen mastic layers as per IS 7198.

11Protection of Damp-Proofing Membrane▼

Protection of Damp-Proofing Membrane (IS 7198)

Key Specifications & Procedures

  • Surface Preparation (6.1.1.6):

    • Keep surface dry during laying.
    • Follow IS 3067-1966 for laying procedures.
    • Continue dewatering until bitumen mastic hardens and structure gains strength to resist hydrostatic pressure.
  • Walls & Floors Above Ground (6.1.2):

    • Damp-proofing must cover full wall thickness (excluding plaster) or base of cavity walls.
    • No setback for pointing.
    • Continuity of bitumen mastic between wall and adjacent floors is mandatory.
    • Provide vertical damp-proof course on inner wall surface (see Fig. 2).
  • Externally Applied Tanking (6.1.3):

    • Minimum 0.6 m working space outside walls.
    • Provide a 100 mm thick, even, structurally sound base, extending 150 mm beyond wall edges for angle fillet (Fig. 3).
    • Cover horizontal mastic asphalt immediately with 50 mm cement-sand screed to avoid damage.
    • Protect vertical damp-proofing by erecting a 10 cm brick wall outside.
    • Protect angle fillet with 50 mm cement-sand screed over building paper.

Typical Dimensions from Figures

ElementDimension
Base concrete thickness100 mm
Base concrete extension150 mm beyond wall
Cement-sand screed cover50 mm
Brick wall protection10 cm thick
Minimum working space0.6 m

Summary Diagram (Fig. 3 - External Tanking Protection)

graph TD
  A[Structural Wall] --> B[Bitumen Mastic Vertical DPC]
  B --> C[10 cm Brick Wall Protection]
  C --> D[5 cm Cement-Sand Screed]
  D --> E[Hard Working Platform (Rubble Soling, Rammed Earth)]
  A --> F[100 mm Lean Base Concrete]
  F --> G[150 mm Extension for Angle Fillet]
  G --> B

Important Notes

  • Maintain continuity of damp-proof
12Special Treatments Around Openings and Penetrations▼

Special Treatments Around Openings and Penetrations (IS 7198)

Key Provisions:

  • Avoid openings for pipes/cables in tanked walls or floors where possible (Clause 6.1.1.5).
  • If essential, provide special treatment around openings as per Fig. 1:
    • Ensure continuity of tanking by sealing and wrapping the opening.
    • Use bitumen mastic or suitable waterproofing material tightly around penetrations.

Damp-Proofing in Walls and Floors Above Ground (Clause 6.1.2):

  • Damp-proofing must cover full wall thickness (excluding plaster).
  • Must be continuous with bitumen mastic layer in floors.
  • Provide vertical damp-proof course on inner wall surface (see Fig. 2).

Externally Applied Tanking (Clause 6.1.3):

  • Minimum 0.6 m working space outside walls.
  • Provide a 100 mm thick sound base, extending 150 mm beyond wall edges for angle fillet (Fig. 3).
  • Protect horizontal mastic asphalt with 50 mm cement-sand screed.
  • Vertical damp-proofing protected by brick wall and screed.

Typical Details:

ComponentThickness/Dimension
Base concrete≥ 100 mm
Base extension beyond wall≥ 150 mm
Cement-sand screed50 mm
Brick wall protection100 mm
Working space outside wall≥ 0.6 m

Visual Summary (Simplified):

flowchart TB
    A[Wall/Floor with Opening] --> B[Seal opening with bitumen mastic]
    B --> C[Wrap pipe/cable tightly]
    C --> D[Ensure continuity of tanking]
    D --> E[Apply vertical DPC on inner wall]
    E --> F[Externally: Provide base concrete ≥100mm]
    F --> G[Extend base 150mm beyond wall edge]
    G --> H[Apply bitumen mastic angle fillet]
    H --> I[Protect with 50mm cement-sand screed]
    I --> J[Protect vertical tanking with brick wall]

References:

  • IS 7198 Clause 6

Popular Questions About IS 7198

?What types of structures can be effectively damp-proofed using bitumen mastic as per IS 7198?▼

IS 7198 specifies the use of bitumen mastic as an effective damp-proofing material primarily for:

  • Walls, floors, and foundations below ground level to prevent moisture ingress.
  • Structures requiring a continuous impervious membrane to block rising damp through capillarity.
  • Building elements exposed to hydrostatic pressure, provided dewatering and curing are properly managed (Clause 6.1.1.6).

Typical Structures Suitable for Bitumen Mastic Damp-Proofing:

  • Basements and underground walls
  • Foundations and plinths
  • Retaining walls
  • Floors at or below ground level
  • Water tanks and reservoirs (internally applied tanking)

Key Notes:

  • Surface must be dry during application.
  • Dewatering must continue until the bitumen layers harden and the structure gains strength.
  • Protective screeds (e.g., 5 cm cement-sand) are recommended over the bitumen layer for durability.
Loading diagram…

This ensures effective damp-proofing against ground moisture and hydrostatic pressures.

?What are the recommended thicknesses and number of coats for bitumen mastic application?▼

According to IS 7198 Clause 8.1 and 8.2, the recommended thickness and number of coats for bitumen mastic application are:

Surface TypeNumber of CoatsTotal Thickness (mm)Notes on Application
Walls and floors above ground level1Minimum 10Single coat
Vertical surfaces & surfaces steeper than 30° below ground level3Minimum 20First coat thin as adhesive; subsequent coats with wooden float
Horizontal & sloping surfaces (≤ 30°) below ground level3Minimum 30Each coat spread evenly with a float

Additional application tips (Clause 8.2):

  • First coat acts as adhesive and prevents blowing.
  • Apply subsequent coats as soon as possible to avoid dust.
  • Use metal trowel for first coat on vertical surfaces; wooden float for others.
  • Protect horizontal mastic with 50 mm cement-sand screed (1:4 ratio) after laying.

This ensures proper waterproofing and durability of the bitumen mastic layer.

?How should surfaces be prepared before applying bitumen mastic for damp-proofing?▼

Surface Preparation Before Applying Bitumen Mastic (IS 7198)

  • Cleanliness: The surface must be thoroughly cleaned of dirt and dust (Clause 6.1.1.2).
  • Dryness: Keep the surface dry during application; continue dewatering until mastic hardens and structure gains strength (Clause 6.1.1.6).
  • Smoothness & Uniformity:
    • Concrete base should have no ridges, indentations, or irregularities (Clause 6.1.1.1).
    • For masonry walls, apply a smooth plaster coat before mastic.
  • Excavation & Protection:
    • Provide a 300 mm space outside walls to keep them dry during laying (Clause 6.1.4a).
    • Keep outside walls clear of earth until vertical mastic coats harden (Clause 6.1.4c).
    • After horizontal mastic and angle fillets, apply a 50 mm cement-sand screed (1:4) for protection (Clause 6.1.4d).

Summary Diagram of Surface Prep Steps

Loading diagram…

This ensures a uniform, durable damp-proofing membrane as per IS 7198 requirements.

?What precautions are necessary for internal and external tanking using bitumen mastic?▼

Precautions for Bitumen Mastic Tanking (IS 7198)

Internal Tanking (Clause 6.1.4)

  • Provide 300 mm clearance outside wall during excavation to keep wall dry.
  • Ensure even base slab surface before applying damp-proofing.
  • Build walls to full height before starting mastic application.
  • Keep outside walls free from earth until 3 vertical mastic coats and loading coats harden (see Fig. 4).
  • After horizontal mastic and angle fillets, apply 50 mm cement-sand screed (1:4) to protect bitumen mastic before structural floor/walls.

External Tanking (Clause 6.1.3)

  • Maintain minimum 0.6 m working space outside walls.
  • Provide a structurally sound base ≥100 mm thick, extending 150 mm beyond wall edges for angle fillet (Fig. 3).
  • Cover horizontal mastic immediately with 50 mm cement-sand screed to prevent damage.
  • Protect vertical damp-proofing by erecting a brick wall immediately after application.

Thickness (Clause 8.1)

Surface TypeNumber of CoatsTotal Thickness
Above ground walls & floors1≥10 mm
Vertical & >30° slope below ground3≥20 mm
Horizontal & ≤30° slope below ground3≥30 mm

Loading diagram…

Summary: Keep surfaces dry and clean, provide adequate working space, apply correct thickness in specified coats, and protect bitumen mastic immediately with cement-sand screed and physical barriers.

?How does IS 7198 address treatment around pipes and service openings in damp-proofing?▼

IS 7198 addresses treatment around pipes and service openings in damp-proofing as follows:

  • Avoid openings for pipes, cables, etc., in tanked walls or floors wherever possible (Clause 6.1.1.5).
  • If openings are essential, special treatment must be applied around them to maintain the continuity of the tanking. This is illustrated in Fig. 1, which shows a typical damp-proofing arrangement around a pipe through an opening.
  • The treatment ensures a sealed, continuous barrier preventing water ingress at these vulnerable points.
  • Additionally, surfaces must be kept dry during laying, and proper dewatering must continue until the bitumen mastic hardens and the structure gains strength (Clause 6.1.1.6).

Summary Diagram (Conceptual):

Loading diagram…

This ensures the damp-proofing layer remains continuous and effective around service penetrations.

✦

Need Detailed Clause Answers?

Ask AI about any clause, requirement, or provision in IS 7198. Get instant, clause-cited responses powered by our indexed library.

Free tier includes 150 queries (50 AI + 100 Reference) · No credit card required